Interfacial microstructure and mechanical property of Ti6Al4V/A6061 dissimilar joint by direct laser brazing without filler metal and groove
- 20 September 2012
- journal article
- Published by Elsevier BV in Materials Science and Engineering: A
- Vol. 560, 111-120
- https://doi.org/10.1016/j.msea.2012.09.044
Abstract
No abstract availableKeywords
This publication has 19 references indexed in Scilit:
- Improving interfacial reaction nonhomogeneity during laser welding–brazing aluminum to titaniumMaterials & Design (1980-2015), 2011
- Joining mechanism of Ti/Al dissimilar alloys during laser welding-brazing processJournal of Alloys and Compounds, 2011
- Dissimilar Metal Joining of 2024 and 7075 Aluminium Alloys to Titanium Alloys by Friction Stir WeldingMATERIALS TRANSACTIONS, 2011
- Diffusion bonding of Al7075 to Ti–6Al–4V using Cu coatings and Sn–3.6Ag–1Cu interlayersJournal of Alloys and Compounds, 2010
- Si diffusion behavior during laser welding-brazing of Al alloy and Ti alloy with Al-12Si filler wireTransactions of Nonferrous Metals Society of China, 2010
- Laser processing of aluminum–titanium-tailored blanksOptics and Lasers in Engineering, 2005
- Microstructure and bonding mechanism of Al/Ti bonded joint using Al–10Si–1Mg filler metalMaterials Science and Engineering: A, 2003
- Formation of a crack-free joint between Ti alloyand Al alloy by using a high-power CO2 laserJournal of Materials Science, 1997
- Electron structure and properties of intermetallic compounds in titanium‐metal dissimilar jointsWelding International, 1995
- Intermetallic compounds formed during brazing of titanium with aluminium filler metalsJournal of Materials Science, 1988