Removal of magnesium from nickel laterite leach liquors by chemical precipitation using calcium hydroxide and the potential use of the precipitate as a filler material
- 31 January 2005
- journal article
- Published by Elsevier BV in Hydrometallurgy
- Vol. 76 (1-2), 105-114
- https://doi.org/10.1016/j.hydromet.2004.09.007
Abstract
No abstract availableKeywords
This publication has 8 references indexed in Scilit:
- Process for the recovery of cobalt and nickel in the presence of magnesium and calcium from sulphate solutions by Versatic 10 and Cyanex 272Minerals Engineering, 2004
- Oxidative precipitation of manganese with SO2/O2 and separation from cobalt and nickelHydrometallurgy, 2002
- Interfacial modification of polypropylene composites filled with magnesium hydroxideJournal of Materials Science, 1995
- Precipitation of Magnesium Hydroxide from BrineIndustrial & Engineering Chemistry Research, 1995
- The rapid precipitation of magnesium hydroxide from aqueous solutions: Analysis of nucleation and crystal growth kinetics, final nucleus numbers and primary crystal sizesCrystal Research and Technology, 1985
- Effect of pH on the growth of Mg(OH)2 crystals in an aqueous environment at 60°CJournal of Crystal Growth, 1977
- The growth of Mg(OH)2 crystals from MgCI2 and Ca(OH)2 in a brine environmentJournal of Crystal Growth, 1977
- The crystallization of magnesium hydroxideDesalination, 1973