Hydrogen-Induced Deformations of Metals Followed by in Situ Scanning Tunneling Microscopy. Palladium Electrolytic Hydrogen Charging and Discharging in Alkaline Solution
- 15 December 1998
- journal article
- research article
- Published by American Chemical Society (ACS) in Langmuir
- Vol. 15 (1), 1-5
- https://doi.org/10.1021/la980633f
Abstract
No abstract availableKeywords
This publication has 11 references indexed in Scilit:
- Scanning Tunneling Microscopy In Situ Observation of Phase-Selective Cathodic Hydrogenation of a V-Ti-Ni-Based Multiphase Alloy ElectrodeElectrochemical and Solid-State Letters, 1999
- The insertion/extraction of deuterium (hydrogen) at Pd sheet electrodes in D2O(H2O) + LiOD(LiOH) electrolyteJournal of Electroanalytical Chemistry, 1996
- Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fractureMaterials Science and Engineering: A, 1994
- Hydrogen interactions with defects in crystalline solidsReviews of Modern Physics, 1992
- Electrochemical study of hydrogen absorption in polycrystalline palladiumJournal of Electroanalytical Chemistry and Interfacial Electrochemistry, 1991
- Proton migration and water diffusion in polyanilineJournal of Electroanalytical Chemistry and Interfacial Electrochemistry, 1989
- Hydrogen embrittlement of α titanium: In situ tem studiesActa Metallurgica, 1988
- Direct observations of hydrogen enhanced crack propagation in ironScripta Metallurgica, 1984
- Hydrogen embrittlement of Nb I—Macroscopic behavior at low temperaturesActa Metallurgica, 1977
- Equilibrium aspects of hydrogen-induced cracking of steelsActa Metallurgica, 1974