Do total hip arthroplasty polyethylene liners without free radicals oxidize in vivo or ex vivo?
- 11 December 2021
- journal article
- research article
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 110 (5), 1113-1119
- https://doi.org/10.1002/jbm.b.34985
Abstract
Crosslinking substantially reduces the wear of ultra-high molecular weight polyethylene (UHMWPE) used in total hip arthroplasty (THA) but some reports have indicated that first generation liners manufactured without antioxidants may be vulnerable to in vivo oxidation. This study evaluated maximum oxidation using Fourier transform infrared spectroscopy per ASTM F2102-06ε1 and linear head penetration using a coordinate measuring machine among 66 revision-retrieved THA components with in vivo durations ranging from 0.02 to 24.6 years. These included 30 liners crosslinked with 5 Mrad of gamma radiation and then melted, 13 non-crosslinked, never-irradiated liners sterilized with gas plasma and 23 non-crosslinked, never-irradiated liners sterilized with ethylene oxide. All liners were vacuum-sealed and stored at −20°C prior to analysis with the exception of three retrievals of each material type that were stored in air for 9.9 to 21.5 years. All 57 vacuum-sealed and frozen retrievals demonstrated good oxidative stability with maximum oxidation indices (OIs) less than 1.0 and 75% (43/57) of these liners had maximum OIs less than 0.1. Linear penetration measurements were lower in the crosslinked liners compared to non-crosslinked retrievals. Although instances of oxidation and embrittlement were found after ex vivo storage in air among liners that did not have free radicals at the time of implantation, in vivo oxidation does not appear to be a clinical concern through the first decade of service for crosslinked liners and at up to 25 years after surgery for non-crosslinked liners.Keywords
Funding Information
- Inova Health System
This publication has 28 references indexed in Scilit:
- Do First-generation Highly Crosslinked Polyethylenes Oxidize In Vivo?Clinical Orthopaedics and Related Research, 2011
- Cross-linked Compared with Historical Polyethylene in THA: An 8-year Clinical StudyClinical Orthopaedics and Related Research, 2008
- In Vivo Oxidation of γ-Barrier–Sterilized Ultra–High-Molecular-Weight Polyethylene BearingsThe Journal of Arthroplasty, 2007
- In Vivo Oxidation of Retrieved Cross-linked Ultra–High-Molecular-Weight Polyethylene Acetabular Components with Residual Free RadicalsThe Journal of Arthroplasty, 2006
- The effect of real-time aging on the oxidation and wear of highly cross-linked UHMWPE acetabular linersBiomaterials, 2006
- Comparison of Cross-Linked Polyethylene Materials for Orthopaedic ApplicationsClinical Orthopaedics and Related Research, 2003
- Advances in the processing, sterilization, and crosslinking of ultra-high molecular weight polyethylene for total joint arthroplastyBiomaterials, 1999
- Development of an extremely wear‐resistant ultra high molecular weight polythylene for total hip replacementsJournal of Orthopaedic Research, 1999
- Gamma sterilization of UHMWPE articular implants: an analysis of the oxidation problemBiomaterials, 1996
- Challenge to the concept that UHMWPE acetabular components oxidize in vivoBiomaterials, 1993